why loss of strength in concrete in 7 days cube test i am
not geting mim 7 days strength that is 67 percent for M-35
and my mix design is perfect there is no doughty,and my
results are near to 7days percentage but not 67 percent.
Answers were Sorted based on User's Feedback
Answer / sjtbehera
what you sure about your mixing. you check slump test, you
check bulkage of sand, you check waste of cement while
mixing, you check compaction factor, if this is right then
result is not obtained please contact Indian standard Buero.
| Is This Answer Correct ? | 12 Yes | 1 No |
Answer / bhauso mane
there are many reasons of concrete failure result as bellow
1)water to cement ratio - increasing water cement ratio
decreases the strength of concrete.
2)quality of cement- firstely check the quality of cement .
3)raw material properties like silt in sand,flaky,
elogation,& hardness of aggregate.
4)mixing & sampling of concrete.
5)compaction & curing of cubes.
6)test machine accuracy.
| Is This Answer Correct ? | 9 Yes | 0 No |
Answer / v.purushotham
The fallowing check points to be done:
 In between interval you should check the mix ratio
i.e. volume/ weight of material,
 Check cement ratio,
 Check slump while pouring the concrete,
 Check the proper mixing of concrete,
 Check the procedure of filling and compacting of
cube mould,
 Check the bulkage of sand,
 Check the gradation of material every 15/ 30 days
interval and compare the designed materials properties,
 Last but not least check the proper curing of
concrete cubes.
| Is This Answer Correct ? | 6 Yes | 0 No |
Answer / saeng
concret will get its 100% characteristic strength after 1
year only.
| Is This Answer Correct ? | 2 Yes | 8 No |
what is lap length?
How is improve my knowledge in construction industries....
what is meant by skyscapers?
What is the thumb rule for calculating the number of chairs in slab?
How to calculate quanty of steel in four leg stirrups?
Please tell me the quantity of cement, sand, flyash, foaming agent required for 1 cubic meter of cellular lightweight concrete blocks. also , is there any admixtures required for the CLC blocks production.
what is the formula to calculate isolated footing
how do you calculate cubic meter to brass
what is the max. dia of steel can be used in open footings?
What is the maximum cement content allowed in RCC?
How to do base isolation for RC framed structure using ETABS software?
what is 3.14 indicates for cutting length of stirrups
Civil Engineering (5086)
Mechanical Engineering (4453)
Electrical Engineering (16638)
Electronics Communications (3918)
Chemical Engineering (1095)
Aeronautical Engineering (239)
Bio Engineering (96)
Metallurgy (361)
Industrial Engineering (259)
Instrumentation (3014)
Automobile Engineering (332)
Mechatronics Engineering (97)
Marine Engineering (124)
Power Plant Engineering (172)
Textile Engineering (575)
Production Engineering (25)
Satellite Systems Engineering (106)
Engineering AllOther (1379)