rasio for outer plaster thickness for wall
Answers were Sorted based on User's Feedback
Answer / varun lekshman
1:4 15mm TK IS GOOD FOR OUR CLIMAT(INDIA)
INSIDE WALL 1:4 12MM TK GOOD
CEILING 1:3 9MM TK GOOD
BUT THE MAIN THING DEPENDS ON COMPANY STANTARD AND PROFIT
| Is This Answer Correct ? | 4 Yes | 2 No |
Answer / saurabh pandey
1:6 in commercial purpose
1:4 in domestic purpose
these r different in order to maintain cost of the project.
| Is This Answer Correct ? | 1 Yes | 0 No |
Answer / satya.mvvs
20 mm thick shall be preferred in rainey area / wetted area
Generally 12mm is preferrable
| Is This Answer Correct ? | 0 Yes | 0 No |
how many cement use for 1cum concrete for 25Grade.
WHAT IS MEANT BY ZERO VALUE IN QUANTITY SURVEYING
States some of the tool bars used in cad?
WHAT IS NON DESTRUCTIVE TEST?PLEASE GIVE ME THE PROCEDURE?
how would you describe yourself and your ideal job
It needs contour survey before plastering a wall / column & floor tiles setting to get––
why we can use dust in concrete insted of fly ash
How to test the quality of Ready Mix M20 concrete (1:1.5:3) before casting at site when lorry arrives? Are there any methods?
in steel bar weight formula (d^2/162).so what is 162.
mix design of concrete using indian standard methods
How to find the requirement of cement and sand for the 1cum of rr masonry work
What is the Allowable silt content of sand for construction purposes?
Civil Engineering (5086)
Mechanical Engineering (4453)
Electrical Engineering (16638)
Electronics Communications (3918)
Chemical Engineering (1095)
Aeronautical Engineering (239)
Bio Engineering (96)
Metallurgy (361)
Industrial Engineering (259)
Instrumentation (3014)
Automobile Engineering (332)
Mechatronics Engineering (97)
Marine Engineering (124)
Power Plant Engineering (172)
Textile Engineering (575)
Production Engineering (25)
Satellite Systems Engineering (106)
Engineering AllOther (1379)