for concrete cubes samples.. what if the 7 days gain the
strength of 42.34 mm/2 and the 28 days only gain the strength
of 37.5 mm/2?
Answers were Sorted based on User's Feedback
Answer / vikranth geddam
sampling and curing for 7 days might be correct. And for 28 days sampking might not be done correctly and at the same time curing also.
| Is This Answer Correct ? | 1 Yes | 0 No |
Hollow block masonry in cement mortar 1:4, 40×20×20cms in superstructure take 10sqm.I want calculation of brick sand
You have casted a column above your footing, and you found out it is off its location by 5cm. What would you Do?
satart to end steps by step process of building construction...? i want to planning theme accuretly
What is the ratio of cement,sand,aggregate of mix m25
how much cement consumption in box type waterproofing
what is the percentage of binding wire required for 1 mt of steel binding in gerally
what are the different types of sizes of bricks?
what is bitumen emultion where it is use
Advantage of Aluminum form work in terms of activities can be skip and cost too
how much need sand and cement for 1 cft roof construction?
0 Answers Indus Valley Construction IVCC,
why we always consider Bulkage due to the voids only for the Fine aggregates not for the Coarse aggregates
Ehat slump test of column & retaing wall.
Civil Engineering (5086)
Mechanical Engineering (4456)
Electrical Engineering (16639)
Electronics Communications (3918)
Chemical Engineering (1095)
Aeronautical Engineering (239)
Bio Engineering (96)
Metallurgy (361)
Industrial Engineering (259)
Instrumentation (3014)
Automobile Engineering (332)
Mechatronics Engineering (97)
Marine Engineering (124)
Power Plant Engineering (172)
Textile Engineering (575)
Production Engineering (25)
Satellite Systems Engineering (106)
Engineering AllOther (1379)