Answer / monti
For 45 degree bend deduct 1d.
For 90 degree bend deduct 2d.
d= dia of bar.
| Is This Answer Correct ? | 22 Yes | 4 No |
Answer / pankaj tandon
monti do you have any IS code for prove this bending procedure
| Is This Answer Correct ? | 0 Yes | 1 No |
1m square 20mm plastering how much of water need curing work
what is a weight of 10mm, 20mm, 40mm aggregate ?
How to take measurement of plastering beam and column.
important question on stones
whether earth to the height of 80cm could be filled in the basement inm place of jamuna sand
# 1, What should be the Maximum Water observation of wood # 2. Is Alluminium is an alloy or not
Is it necessary to apply tack coat over the primecoat. IF not what happens.answers other than 1.to superimpose the next layer(2) to adhere the layers so as to form homogenity.
Why we use pcc in foundation?
why we use 19x9x9and 20x10x10 but not other
how to calculate sump capacity
2 Answers AVS, KMC, Personal Assistant, Shrey Associates,
How to calculate the sand and aggregate in concrete
what is tensile strength?
Civil Engineering (5086)
Mechanical Engineering (4456)
Electrical Engineering (16639)
Electronics Communications (3918)
Chemical Engineering (1095)
Aeronautical Engineering (239)
Bio Engineering (96)
Metallurgy (361)
Industrial Engineering (259)
Instrumentation (3014)
Automobile Engineering (332)
Mechatronics Engineering (97)
Marine Engineering (124)
Power Plant Engineering (172)
Textile Engineering (575)
Production Engineering (25)
Satellite Systems Engineering (106)
Engineering AllOther (1379)