why we leave expansion joint between to complex
Answers were Sorted based on User's Feedback
Answer / anil kumar prasad
To prevent the developement of crack due to expansion &
contraction of steel & cement with temperature.
| Is This Answer Correct ? | 4 Yes | 0 No |
Answer / rishabh thakur
absolutly right, i am agree with Mr. sunil, bcz the material used(cement ,fine etc.) expand with temp.so it should be provided b/w to complex
| Is This Answer Correct ? | 4 Yes | 3 No |
In which year onward limit state method used in india...
What is the use of mirror command?
what will be the quantity of matterial and water for pcc in 1 cubic meter , the ratio is 1:4:8 (cement:sand:aggr) ?
How do you calculate the mix ratio of concrete i.e. what is the cement:sand:agrugate ratio in 20Mpa, 21Mpa, 22Mpa etc...
In Fe415 & Fe500,What is mean by "Fe" and "415/500"?
12 Answers CMR, Modi Builders, Taehwa Enterprises, vvip,
What is the main difference between crushing test and impact test in coarse aggregate?
Define What is the force exerted by the Tacoma narrows bridge?
What is the maximum allowable 'Silt content' in River sand
16 Answers IVRCL, Om Buildcon,
Why are pull-out tests performed for soil nails?
what is the diferance np3 and np4 pipe
1 Answers Sharda Construction,
how do we calculate wastage of steel in the site,what r the items to taken into account for wastage calculation?
Suppose a new brick wall is being constructed,and the courses and not aligned horizontally,what negetives can it cause?
Civil Engineering (5086)
Mechanical Engineering (4456)
Electrical Engineering (16639)
Electronics Communications (3918)
Chemical Engineering (1095)
Aeronautical Engineering (239)
Bio Engineering (96)
Metallurgy (361)
Industrial Engineering (259)
Instrumentation (3014)
Automobile Engineering (332)
Mechatronics Engineering (97)
Marine Engineering (124)
Power Plant Engineering (172)
Textile Engineering (575)
Production Engineering (25)
Satellite Systems Engineering (106)
Engineering AllOther (1379)