What is the density of Cement, Fly ash,20 mm aggregate, 10
mm aggregate and stone dust?
Answer Posted / sukhwinder singh
cement density-1440kg/cum
10MM-1600kg /cum
20MM-1700kg/ cum
Dry sand-1650kg/cum
Stone dust-1750kg/cum
Fly ash-750kg/cum
Water-
Is This Answer Correct ? | 20 Yes | 2 No |
Post New Answer View All Answers
Method of findingthe dry ingredient quantity of 1 m3 concrete. what is the difference between static and dynamic induced emf? Testing charges bill given for Rs. 32,000/- but not added service tax in this bill. So, How much TDS will be deduct
Pls provide me with the calculation or codes related to de- shuttering of flat slabs
What are new methods /technologies of pothole patching?
is it fair to recruit another prestressing agency once earlier agency has provided guide cone for post stressing the Concrete -I girders? It is observed that the bearing plate of another agency is not matching with the earlier one resulting in protruded strands after stressing from the face of girder. Kindly advice.
crank types
Can we use concrete of slump cone in cube casting in which we have already measured slump?
what is right & short method of measurement of slab&beam
As per Kandal suggestions, we have implemented rolling starts on 140 (+/- 5) degrees and we kept 3 rollars to complete the rolling before falling 125 degrees and the Aggregate AIV is below 22. But When the DBM bed is being rolled 3rd high viabration, (Before 1 plain & low ,2 high Viabrations), the aggregate is getting sharp edge agg. projections are damaged. As the literature is said that, the VG-30 Grade having better control the temp. susceptibility than Penetration grade. if so we could not get this problem at site. But we are facing on site. let me know.
List out some of the software used in the construction sector to estimate cost and monitoring expenses?
How do you measure concrete?
How much cements bag (or in KG) required for 1 Sq. M concrete, for M-30 grad concrete as per CPWD and where is thr proof on site
what motivates you to do a good job
What is demising walls?
why development length = 50D . why not 100D
important question on stones