what is the process of repair the structure in whitch
reinforcement is open
Answer Posted / sumit
That situation shoe is honeycombing
So he is repaired with a mix of Nitobond & cement & water
If honeycombing is visible in big area then Jacketing
Method Applied (If possible)
| Is This Answer Correct ? | 2 Yes | 2 No |
Post New Answer View All Answers
what is grade intersection?
What things architect have to take care of before starting any project?
What is the maximum crushing load in Kg & crushing strength in N/mm2 for M25 & M 15 Grade concrete
What is the use of water table & Kreb stone for drain
Difference between pre-tensioning and post-tensioning.
What is factor not to be taken in consideration in mix design?
Journal entry Gross salary 10000 Tax 1000 Employee contribution 2000 Employer contribution 2000
how to design and calculate materail quantity for concrete speedbreaker ?
how we can find sieve #4 is 4.75mm?
how to Concrete cubes testing curing time 7 days casting date 24.05.17 testing date ?
how to calculate the crushing strength of cement concrete paver blocks 100x100x60 mm thich.
Coverage of 25mm.thick ratio of 1:4 cement mortar?
At what point does a circle start losing area when being flattened?
Describe the advantages and disadvantages of using plastic and timber fenders?
If we buy crush sand for 3200/ Brass and cement for Rs350 /Bag and flyash 1200 / tonne....and my production is 230 Bricks per bag than how much cost is required for 1 flyash brick?